BOROALUMINOSILICATE GLASS COMPOSITION HAVING HIGH FUSION FLOW RATE AND ADVANTAGED PAIR SHAPING TEMPERATURE

Abstract: disclosed herein are embodiments of a glass composition including about 55 mol % to about 67 mol % sio, about 10 mol % to about 13 mol % bo, about 11 mol % to about 15 mol % alo, and about 12 mol % to about 16 mol % alkali oxide. in one or more embodiments, the glass composition comprises a temperature at which a viscosity of the borosilicate glass composition is 10p from about 630� c. to about 650� c. also disclosed is a method of forming a glass ply. in the method, a trough in an isopipe is overflowed with at least two streams of the glass composition, and the at least two streams of the glass composition are fused at a root of the isopipe to form the glass ply. the glass ply can be pair-shaped to form laminates for use as automotive glazing.

Inventor(s): Timothy Michael Gross, Aaron Joshua Hade, Chunhong Chelsie He, Jian Luo

CPC Classification: C03C3/091 (CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS)

Search for rejections for patent application number 20250187971


Cookies help us deliver our services. By using our services, you agree to our use of cookies.