Jump to content

20250171319. Porous Spherical Silica, (TOKUYAMA)

From WikiPatents

POROUS SPHERICAL SILICA, CATALYST CARRIER, COSMETIC, ANALYTICAL COLUMN, POLISH, RESIN COMPOSITION, AND METHOD OF PRODUCING POROUS SPHERICAL SILICA

Abstract: provided are an independent porous spherical silica such that the alkali metal content is reduced, the hardness of the particles is increased, and the number of shred particles is reduced; and a method of producing such a silica. in the porous spherical silica, the diameter (d50) of volume based particle size distribution is 2 �m to 200 �m, the ratio (d10/d90) of the diameter (d10) to the diameter (d90) is at least 0.3, the pore volume is 0.5 to 8 ml/g, the mode pore radius is 5 to 50 nm, the specific surface area is 50 to 400 m/g, and the arithmetic mean value of “compressive test forces when specimens are found to break” obtained according to jis z8844 is 1.0�10to 2.0�10mn, the number of particles each having a circularity of at most 0.7 is at most 20, and the alkali metal content is at most 50 ppm.

Inventor(s): Noriko YOSHIMURA

CPC Classification: C01B33/186 (Preparation of finely divided silica neither in sol nor in gel form; After-treatment thereof (preparation of aerogels by dehydrating gels ; treatment to enhance the pigmenting or filling properties ))

Search for rejections for patent application number 20250171319


Cookies help us deliver our services. By using our services, you agree to our use of cookies.