OPTICAL FIBER AND OPTICAL FIBER RIBBON
Organization Name
Sumitomo Electric Industries, Ltd.
Inventor(s)
Noriaki Iwaguchi of Osaka-shi, Osaka (JP)
Miho Ikegawa of Osaka-shi, Osaka (JP)
OPTICAL FIBER AND OPTICAL FIBER RIBBON - A simplified explanation of the abstract
This abstract first appeared for US patent application 18279474 titled 'OPTICAL FIBER AND OPTICAL FIBER RIBBON
The abstract describes an optical fiber with a glass fiber core, cladding, and a coating resin layer. The primary resin layer contains a silicone (meth)acrylate and a photopolymerization initiator, while the secondary resin layer contains a urethane (meth)acrylate and a photopolymerization initiator. The coating resin layer has a low tin content of 150 ppm or less.
- Glass fiber core with cladding and coating resin layer
- Primary resin layer with silicone (meth)acrylate and photopolymerization initiator
- Secondary resin layer with urethane (meth)acrylate and photopolymerization initiator
- Low tin content of 150 ppm or less in the coating resin layer
Potential Applications: - Telecommunications - Data transmission - Fiber optic networks
Problems Solved: - Enhanced durability of optical fibers - Improved signal transmission quality
Benefits: - Increased reliability - Reduced signal loss - Extended lifespan of optical fibers
Commercial Applications: Title: Enhanced Optical Fiber Coating for Improved Signal Transmission This technology can be utilized in telecommunications, data centers, and internet service providers to enhance signal transmission quality and reliability in fiber optic networks.
Questions about Enhanced Optical Fiber Coating: 1. How does the low tin content in the coating resin layer benefit the optical fiber? - The low tin content helps improve the overall performance and longevity of the optical fiber by reducing potential signal interference. 2. What are the main differences between the primary and secondary resin layers in the coating of the optical fiber? - The primary resin layer contains silicone (meth)acrylate, while the secondary resin layer contains urethane (meth)acrylate, each serving specific purposes in enhancing the optical fiber's properties.
Original Abstract Submitted
An optical fiber comprises a glass fiber including a core and a cladding, and a coating resin layer for coating the glass fiber; the coating resin layer has a primary resin layer in contact with the glass fiber for coating the glass fiber, and a secondary resin layer for coating the primary resin layer; the primary resin layer includes a cured product of a first resin composition containing a silicone (meth)acrylate and a photopolymerization initiator; the secondary resin layer includes a cured product of a second resin composition containing a urethane (meth)acrylate and a photopolymerization initiator; and the amount of tin contained in the coating resin layer is 150 ppm or less in a mass ratio.