18589656. STRETCH BLOW-MOLDED ARTICLE AND METHOD FOR PRODUCING STRETCH BLOW-MOLDED ARTICLE simplified abstract (CANON KABUSHIKI KAISHA)
Contents
STRETCH BLOW-MOLDED ARTICLE AND METHOD FOR PRODUCING STRETCH BLOW-MOLDED ARTICLE
Organization Name
Inventor(s)
TSUNENORI Ashibe of Kanagawa (JP)
STRETCH BLOW-MOLDED ARTICLE AND METHOD FOR PRODUCING STRETCH BLOW-MOLDED ARTICLE - A simplified explanation of the abstract
This abstract first appeared for US patent application 18589656 titled 'STRETCH BLOW-MOLDED ARTICLE AND METHOD FOR PRODUCING STRETCH BLOW-MOLDED ARTICLE
Simplified Explanation: The patent application describes a stretch blow-molded article made of two different polyesters with specific intrinsic viscosity values, one of which has a structure corresponding to terephthalic acid and bisphenol A.
Key Features and Innovation:
- Combination of two different polyesters with specific intrinsic viscosity values.
- Unique structure of the second polyester with terephthalic acid and bisphenol A.
- Stretch blow-molded article for specific applications.
Potential Applications: The technology can be used in the production of various packaging materials, containers, and bottles.
Problems Solved:
- Enhanced performance and properties of the stretch blow-molded article.
- Improved structural integrity and durability.
Benefits:
- Increased strength and stability.
- Potential for lightweight and cost-effective packaging solutions.
Commercial Applications: The technology can be utilized in the food and beverage industry, pharmaceuticals, and personal care products for packaging purposes.
Questions about Stretch Blow-Molded Article: 1. How does the combination of two different polyesters enhance the properties of the stretch blow-molded article? 2. What specific advantages does the unique structure of the second polyester bring to the article?
Original Abstract Submitted
A stretch blow-molded article comprising: a first polyester; and a second polyester having a structure different from a structure of the first polyester, wherein an intrinsic viscosity value of the first polyester is 0.60 to 0.74 dL/g, and the second polyester has a structure corresponding to terephthalic acid and a structure corresponding to bisphenol A.