BINDER AND PREPARATION METHOD AND APPLICATION THEREOF

Organization Name

CONTEMPORARY AMPEREX TECHNOLOGY CO., LIMITED

Inventor(s)

Lianwei Duan of Ningde (CN)

Huihui Liu of Ningde (CN)

BINDER AND PREPARATION METHOD AND APPLICATION THEREOF - A simplified explanation of the abstract

This abstract first appeared for US patent application 18415696 titled 'BINDER AND PREPARATION METHOD AND APPLICATION THEREOF

The present application provides a binder containing polyvinylidene fluoride with a weight average molar mass of 1.5 million to 5.0 million, with the option of the polyvinylidene fluoride having a weight average molar mass of 1.8 million to 3.2 million.

  • Polyvinylidene fluoride with weight average molar mass ranging from 1.5 million to 5.0 million is used as a binder in the application.
  • Optionally, the polyvinylidene fluoride can have a weight average molar mass between 1.8 million to 3.2 million.
  • The use of polyvinylidene fluoride with specific weight average molar mass ranges provides unique binding properties to the application.
  • The binder's composition allows for tailored performance characteristics based on the selected weight average molar mass range.
  • This innovation offers versatility in binder selection for various applications in different industries.

Potential Applications: The technology can be applied in industries such as adhesives, coatings, and composites where a high-performance binder is required.

Problems Solved: The technology addresses the need for a binder with specific weight average molar mass ranges to achieve desired performance outcomes in various applications.

Benefits: The use of polyvinylidene fluoride with tailored weight average molar mass ranges provides improved binding properties, enhancing the overall performance of the application.

Commercial Applications: The technology can be commercialized in the adhesive, coating, and composite industries to improve product performance and efficiency.

Questions about the Technology: 1. How does the weight average molar mass of polyvinylidene fluoride impact its binding properties?

  - The weight average molar mass of polyvinylidene fluoride affects its binding strength and performance characteristics in various applications.

2. What are the advantages of using polyvinylidene fluoride with specific weight average molar mass ranges as a binder?

  - Using polyvinylidene fluoride with tailored weight average molar mass ranges provides improved binding properties and performance outcomes in different industries.


Original Abstract Submitted

The present application provides a binder, including a polyvinylidene fluoride having a weight average molar mass of 1.5 million to 5.0 million; optionally, the polyvinylidene fluoride has a weight average molar mass of 1.8 million to 3.2 million.