18589656. STRETCH BLOW-MOLDED ARTICLE AND METHOD FOR PRODUCING STRETCH BLOW-MOLDED ARTICLE simplified abstract (CANON KABUSHIKI KAISHA)

From WikiPatents
Jump to navigation Jump to search

STRETCH BLOW-MOLDED ARTICLE AND METHOD FOR PRODUCING STRETCH BLOW-MOLDED ARTICLE

Organization Name

CANON KABUSHIKI KAISHA

Inventor(s)

TSUNENORI Ashibe of Kanagawa (JP)

YOHEI Doi of Saitama (JP)

STRETCH BLOW-MOLDED ARTICLE AND METHOD FOR PRODUCING STRETCH BLOW-MOLDED ARTICLE - A simplified explanation of the abstract

This abstract first appeared for US patent application 18589656 titled 'STRETCH BLOW-MOLDED ARTICLE AND METHOD FOR PRODUCING STRETCH BLOW-MOLDED ARTICLE

Simplified Explanation: The patent application describes a stretch blow-molded article made of two different polyesters with specific intrinsic viscosity values, one of which has a structure corresponding to terephthalic acid and bisphenol A.

Key Features and Innovation:

  • Combination of two different polyesters with specific intrinsic viscosity values.
  • Unique structure of the second polyester with terephthalic acid and bisphenol A.
  • Stretch blow-molded article for specific applications.

Potential Applications: The technology can be used in the production of various packaging materials, containers, and bottles.

Problems Solved:

  • Enhanced performance and properties of the stretch blow-molded article.
  • Improved structural integrity and durability.

Benefits:

  • Increased strength and stability.
  • Potential for lightweight and cost-effective packaging solutions.

Commercial Applications: The technology can be utilized in the food and beverage industry, pharmaceuticals, and personal care products for packaging purposes.

Questions about Stretch Blow-Molded Article: 1. How does the combination of two different polyesters enhance the properties of the stretch blow-molded article? 2. What specific advantages does the unique structure of the second polyester bring to the article?


Original Abstract Submitted

A stretch blow-molded article comprising: a first polyester; and a second polyester having a structure different from a structure of the first polyester, wherein an intrinsic viscosity value of the first polyester is 0.60 to 0.74 dL/g, and the second polyester has a structure corresponding to terephthalic acid and a structure corresponding to bisphenol A.