18570074. FLUX, SUBSTRATE AND MANUFACTURING METHOD, AND DEVICE simplified abstract (BOE TECHNOLOGY GROUP CO., LTD.)
Contents
FLUX, SUBSTRATE AND MANUFACTURING METHOD, AND DEVICE
Organization Name
BOE TECHNOLOGY GROUP CO., LTD.
Inventor(s)
FLUX, SUBSTRATE AND MANUFACTURING METHOD, AND DEVICE - A simplified explanation of the abstract
This abstract first appeared for US patent application 18570074 titled 'FLUX, SUBSTRATE AND MANUFACTURING METHOD, AND DEVICE
The present disclosure introduces a flux containing a bulk material and a powdery conductive material mixed within it, with a volume ratio of the conductive material to the flux ranging from 5% to 10%.
- The flux consists of a combination of bulk material and powdery conductive material.
- The volume ratio of the conductive material to the flux is between 5% and 10%.
Potential Applications:
- This technology can be applied in the manufacturing of electronic devices.
- It can be used in the production of circuit boards and other electronic components.
Problems Solved:
- Enhances the conductivity of the flux.
- Improves the performance of electronic devices.
Benefits:
- Increased efficiency in electronic device manufacturing.
- Enhanced conductivity for better device performance.
Commercial Applications:
- This technology can be utilized in the electronics industry for the production of various electronic components.
- It can be integrated into the manufacturing processes of electronic devices to improve their overall performance.
Questions about the Technology: 1. How does the addition of the conductive material impact the overall performance of the flux? 2. What are the specific electronic devices that can benefit from the use of this technology?
Frequently Updated Research: There may be ongoing research related to the optimization of the volume ratio of the conductive material in the flux for different applications.
Original Abstract Submitted
The present disclosure provides a flux, a substrate, a manufacturing method thereof, and a device. The flux includes a bulk material and a powdery conductive material mixed in the bulk material, and a volume ratio of the conductive material to the flux is 5% to 10%.