18698564. LAMINATE MATERIAL WITH SUPERIOR BARRIER PERFORMANCE AND PREPARATION METHOD THEREOF (Dow Global Technologies LLC)

From WikiPatents
Revision as of 07:39, 19 December 2024 by Wikipatents (talk | contribs) (Creating a new page)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

LAMINATE MATERIAL WITH SUPERIOR BARRIER PERFORMANCE AND PREPARATION METHOD THEREOF

Organization Name

Dow Global Technologies LLC

Inventor(s)

Gang Wang of Shanghai (CN)

ChenYan Bai of Shanghai (CN)

Zhe Du of Shanghai (CN)

Fanji Wang of Tokyo (JP)

Xiaobing Yun of Shanghai (CN)

Jianping Pan of Shanghai (CN)

Jingyi Xu of Shanghai (CN)

Jianliang Zhu of Shanghai (CN)

Huan Qiu of Shanghai (CN)

LAMINATE MATERIAL WITH SUPERIOR BARRIER PERFORMANCE AND PREPARATION METHOD THEREOF

This abstract first appeared for US patent application 18698564 titled 'LAMINATE MATERIAL WITH SUPERIOR BARRIER PERFORMANCE AND PREPARATION METHOD THEREOF



Original Abstract Submitted

Provided are a laminate material, an article comprising the laminate material and a method for preparing the laminate material. The laminate material, comprises a first substrate comprising at least one metalized PE-based film, a second substrate comprising at least one PE-based film, and an adhesive layer adhering the first substrate to the second substrate, wherein the adhesive layer is derived from a two-component solvent-based polyurethane adhesive composition, and wherein the concentration of fatty acids or fatty acid derivatives in the metalized PE-based film is less than 300 ppm, based on the total weight of the metalized PE-based film. The two-component solvent-based polyurethane adhesive composition comprises a polyester polyol component and a polyisocyanate component, wherein the polyol component has 40 wt %-60 wt % of aromatic rings in the backbone, based on the total weight of the polyester polyol and a Mw between 5.000 and 50.000, and wherein the weight ratio of the polyester polyol component to polyisocyanate component is from 100:5 to 100:30.