POSITIVE ELECTRODE MATERIAL, PREPARATION METHOD THEREOF, AND SECONDARY BATTERY INCLUDING SAME

Organization Name

CONTEMPORARY AMPEREX TECHNOLOGY CO., LIMITED


Inventor(s)

Qiang Chen of Ningde City (CN)


Qi Wu of Ningde City (CN)


Jingpeng Fan of Ningde City (CN)


Tao Huang of Ningde City (CN)


Na Liu of Ningde City (CN)


POSITIVE ELECTRODE MATERIAL, PREPARATION METHOD THEREOF, AND SECONDARY BATTERY INCLUDING SAME - A simplified explanation of the abstract

  • This abstract for appeared for US patent application number 18326025 Titled 'POSITIVE ELECTRODE MATERIAL, PREPARATION METHOD THEREOF, AND SECONDARY BATTERY INCLUDING SAME'

Simplified Explanation

The abstract describes a positive electrode material for batteries. It consists of a core and a shell layer. The core has a molecular formula of LiNiCoMnM1O, where x is between 0.8 and 1.0, y is between 0 and 0.2, a is between 0 and 0.1, z is between 0 and 0.1, and M1 can be Al, Ta, or B. The shell layer has a molecular formula of LiCoA1NbM2O, where m is between 0.85 and 1.0, n is between 0 and 0.15, b is between 0 and 0.1, 1-m-n is between 0.001 and 0.02, c is between 0 and 0.05, and M2 can be W, Mo, Ti, Zr, Y, or Yb.


Original Abstract Submitted

A positive electrode material, including a core and a shell layer are provided. In some embodiments, a molecular formula of the core is LiNiCoMnM1O, 0.8≤x<1.0, 0<y<0.2, 0<a<0.1, 0≤z<0.1, and M1 is selected from at least one of Al, Ta, and B; and a molecular formula of the shell layer is LiCoA1NbM2O, 0.85≤m<1.0, 0<n<0.15, 0<b<0.1, 0.001≤1-m-n≤0.02, 0≤c<0.05, and M2 is selected from at least one of W, Mo, Ti, Zr, Y, and Yb.