US Patent Application 18162745. COMPOSITION, POLYMER PREPARED THEREFROM, AND ELECTRONIC APPARATUS INCLUDING THE SAME simplified abstract

From WikiPatents
Jump to navigation Jump to search

COMPOSITION, POLYMER PREPARED THEREFROM, AND ELECTRONIC APPARATUS INCLUDING THE SAME

Organization Name

Samsung Display Co., Ltd.


Inventor(s)

Sebeen Lee of Yongin-si (KR)

Bookan Ki of Yongin-si (KR)

Hoyun Byun of Yongin-si (KR)

Intae Son of Yongin-si (KR)

Donghyeon Lee of Yongin-si (KR)

Jeongin Lee of Yongin-si (KR)

COMPOSITION, POLYMER PREPARED THEREFROM, AND ELECTRONIC APPARATUS INCLUDING THE SAME - A simplified explanation of the abstract

This abstract first appeared for US patent application 18162745 titled 'COMPOSITION, POLYMER PREPARED THEREFROM, AND ELECTRONIC APPARATUS INCLUDING THE SAME

Simplified Explanation

The abstract describes a composition that includes several monomers, an oligomer, a silane coupling agent, and a photoinitiator. The composition has a specific viscosity range at room temperature.

  • The composition includes a first monomer with a hydroxy group, a second monomer without a hydroxy group, a third monomer with a terminal heterocyclic group, and a fourth monomer with an alkylene glycol.
  • The composition also includes an oligomer, which is a polymer with a small number of repeating units.
  • A silane coupling agent is included in the composition, which helps improve adhesion between different materials.
  • A photoinitiator is also present, which initiates a chemical reaction when exposed to light.
  • The composition has a viscosity between 5 centipoise and 50 centipoise at room temperature, indicating its flow characteristics.


Original Abstract Submitted

A composition including a first monomer including a hydroxy group, a second monomer that does not include a hydroxy group, a third monomer including a terminal heterocyclic group, a fourth monomer including an alkylene glycol, an oligomer, a silane coupling agent, and a photoinitiator. The composition has a viscosity of 5 centipoise to 50 centipoise at about room temperature.